Abstract
This article provides an introduction to architected cellular materials, their design, fabrication, and application domain. It discusses design decisions involving the selection, sizing, and spatial distribution of the unit cell, property-scaling relationships, and the integration of cells within an external boundary. It describes how manufacturing constraints influence achievable feature resolution, dimensional accuracy, properties, and defects. It also discusses the mechanical behavior of architected cellular materials and the role of additive manufacturing in their fabrication.
Dhruv Bhate, Devlin Hayduke, Architected Cellular Materials, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 1–10, https://doi.org/10.31399/asm.hb.v24A.a0006951
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!