Zirconia for Dental Implants
By
Saurabh Gupta
Saurabh Gupta
The International Academy of Ceramic Implantology, Universitat Jaume I, COHO Biotechnology, Clean Implant Foundation
Search for other works by this author on:
-
Published:2022
Abstract
One of the most frequently cited advantages of ceramics in dentistry relates to aesthetics, and the same applies for dental implants. Zirconia has emerged as the material of choice for nonmetal implants. This article introduces the reader to zirconia as an implant material, its properties, manufacturing processes, and the particular surface modifications and treatments that have rendered its surfaces biologically compatible with peri-implant soft and hard tissues.
Topics
Stainless steel,
Piezoelectric ceramics,
Biomaterials,
Dental implant alloys,
Dental cements,
Orthopedic fixation devices,
Orthopedic implants,
Stents,
Tissue scaffolds,
Cobalt powder,
Titanium powder,
Stainless steel powder,
Particle analysis,
Cobalt-chromium alloys,
Titanium alloys,
Zirconia ceramics,
Additive manufacturing,
Modeling tools and methods,
Biological properties,
Piezoelectricity,
Electrochemical properties,
Rheological properties,
Medical instruments,
Solidification,
Medical and biomedical,
Biocompatibility
You do not currently have access to this chapter.
Citation
Saurabh Gupta, Zirconia for Dental Implants, Additive Manufacturing in Biomedical Applications, Vol 23A, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2022, p 479–485, https://doi.org/10.31399/asm.hb.v23A.a0006853
Download citation file:
Related Book Content
Biotribology
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Corrosion Effects on the Biocompatibility of Metallic Materials and Implants
Corrosion: Environments and Industries
Material Aspects of Additively Manufactured Orthopedic Implants of Titanium Alloys
Additive Manufacturing in Biomedical Applications
Biotribology of Medical Implants
Friction, Lubrication, and Wear Technology
Biomaterials
Metals Handbook Desk Edition (2nd Edition)
Introduction to Medical Implant Materials
Materials for Medical Devices
Accepted Practice for Recognizing Artifacts in Air Plasma Spray Thermal Barrier Coating Microstructures
Thermal Spray Technology Accepted Practices
Biocompatibility of Metallic Materials for Medical Devices—The Effects of Corrosion and Corrosion Products
Materials for Medical Devices
Biocompatibility of Polymers
Materials for Medical Devices
Nitriding of Titanium Alloys
Heat Treating of Nonferrous Alloys