Abstract
Bridging the gap between education and medical practice, centralized hospital-based 3D printing, or what is termed point-of-care (POC) manufacturing, has been rapidly growing in the United States as well as internationally. This article provides insights into the considerations and the current workflow of creating 3D-printed anatomical models at the POC. Case studies are introduced to show the complex range of anatomical models that can be produced while also exploring how patient care benefits. It describes the advanced form of communication in medicine. The advantages as well as pitfalls of using the patient-specific 3D-printed models at the POC are addressed, demonstrating the fundamental knowledge needed to create 3D-printed anatomical models through POC manufacturing.
Victoria Sears, Jonathan Morris, Anatomical Modeling at the Point of Care, Additive Manufacturing in Biomedical Applications, Vol 23A, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2022, p 390–401, https://doi.org/10.31399/asm.hb.v23A.a0006896
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.