Stereolithographic Additive Manufacturing of Biological Scaffolds
-
Published:2022
Abstract
Stereolithographic (STL) additive manufacturing (AM) can be used to fabricate practical components. This article discusses the processes involved in STL-AM of biological scaffolds, providing information on bioscaffold processing, cavity arrangements, and microlattice distributions. Within the last topic, the sub-topic of scaffold modulation is discussed.
Soshu Kirihara, Stereolithographic Additive Manufacturing of Biological Scaffolds, Additive Manufacturing in Biomedical Applications, Vol 23A, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2022, p 246–251, https://doi.org/10.31399/asm.hb.v23A.a0006887