This article discusses alginate/gelatin-based bioinks in 3D bioprinting applications, providing a summary of the most relevant previous work in the field. It presents advanced compositions to enhance functionality and/or optimize hydrogels for 3D bioprinting. The article discusses advanced printing techniques for alginate/gelatin-based bioinks.
Sonja Kuth, Faina Bider, Aldo R. Boccaccini, Bioprinting/Biofabrication with Alginate/Gelatin-Based Bioinks, Additive Manufacturing in Biomedical Applications, Vol 23A, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2022, p 353–362, https://doi.org/10.31399/asm.hb.v23A.a0006855