Abstract
This appendix provides reference tables listing weldability of cast irons, steels, and nonferrous metals. A process selection table for arc welding carbon steels is included, and recommended preheat and interpass temperature tables are also presented. This appendix includes information on qualification codes and standards.
You do not currently have access to this chapter.
Citation
Reference Tables, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 365–379, https://doi.org/10.31399/asm.tb.wip.t65930365
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Weldability of Ferrous and Nonferrous Alloys
Welding Fundamentals and Processes
Summary of Fusion Welding Processes
Welding Fundamentals and Processes
Welding of Low-Alloy Steels
Welding, Brazing, and Soldering
Solidification Structures of Steels and Cast Irons
Metallography and Microstructures
Heat Treating of Carbon Steels
Practical Heat Treating (Second Edition)
Brittle Fracture Assessment and Failure Assessment Diagrams
Analysis and Prevention of Component and Equipment Failures
Origin of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Joining Technology and Practice
Titanium: A Technical Guide (Second Edition)
Dip Brazing
Welding, Brazing, and Soldering
Preheat and Postweld Heat Treatment Temperatures for Selected Steels
Welding Fundamentals and Processes