Chapter 11: Corrosion of Weldments[1] Available to Purchase
By
C.E. Cross
C.E. Cross
Martin Marietta Astronautics Group
Search for other works by this author on:
-
Published:1997
Page range:
189 - 196
Abstract
This article describes some of the general characteristics associated with the corrosion of weldments. The role of macrocompositional and microcompositional variations, a feature common to weldments, is emphasized in this article to bring out differences that need to be realized in comparing corrosion of weldments to that of wrought materials. The article discusses the most important methods available to minimize corrosion in weldments.
You do not currently have access to this chapter.
Citation
A. Wahid, D.L. Olson, D.K. Matlock, C.E. Cross, Corrosion of Weldments, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 189–196, https://doi.org/10.31399/asm.tb.wip.t65930189
Download citation file:
Related Book Content
Aqueous Corrosion Failures
Understanding How Components Fail (Third Edition)
Corrosion of Austenitic Stainless Steel Weldments
Corrosion of Weldments
Galvanic Corrosion Failure of Austenitic Stainless Steel Pipe Flange Assemblies
Handbook of Case Histories in Failure Analysis
Corrosion of Carbon Steel Weldments
Corrosion: Fundamentals, Testing, and Protection
Corrosion of Carbon Steel Weldments
Corrosion in the Petrochemical Industry (Second Edition)
Forms of Corrosion
Failure Analysis and Prevention (2021 Edition)
Monitoring and Testing of Weld Corrosion
Corrosion of Weldments
Fatigue Fracture of a Helicopter Tail Rotor Blade Due to Field-Induced Corrosion
Handbook of Case Histories in Failure Analysis
Corrosion in Commercial Aviation
Corrosion: Environments and Industries
Environmentally-Induced Failures
Fatigue and Fracture Understanding the Basics