Skip Nav Destination
ASM Technical Books
Weld Integrity and PerformanceAvailable to Purchase
Edited by
ASM International
ISBN electronic:
978-1-62708-359-1
Publication date:
1997
Book Chapter
Chapter 7: Fatigue and Fracture Control of Welds[1] Available to Purchase
By
-
Published:1997
Page range:
113 - 139
Abstract
This article discusses the various options for controlling fatigue and fracture in welded steel structures, the factors that influence them the most, and some of the leading codes and standards for designing against these failure mechanisms. The two most widely used approaches discussed for fatigue control in welded joints are the S-N curve approach and the fracture mechanics assessment methods.
You do not currently have access to this chapter.
Citation
Tarsem Jutla, Fatigue and Fracture Control of Welds, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 113–139, https://doi.org/10.31399/asm.tb.wip.t65930113
Download citation file:
Related Book Content
Failure of a Steam Accumulator Due to Lack of Complete Weld Penetration
ASM Failure Analysis Case Histories: Processing Errors and Defects
Fatigue and Fracture Control of Weldments
Fatigue and Fracture
Fatigue Cracking of a Stainless Steel Elbow Assembly at a Welded Joint in a High-Stress Region
ASM Failure Analysis Case Histories: Air and Spacecraft
Cathodic Protection
Corrosion in the Petrochemical Industry (Second Edition)
Weld Procedure Qualification
Welding, Brazing, and Soldering
Forming Process Anomalies in Diesel Fuel Injection Control Sleeve
ASM Failure Analysis Case Histories: Automobiles and Trucks
Failure Analysis of Welded Structures
Analysis and Prevention of Component and Equipment Failures
Failures of Bridge Components
Analysis and Prevention of Component and Equipment Failures
Fatigue Fracture of a Type 347 Stainless Steel Pressure-Probe Housing Originating at Voids in a Brazed Joint
ASM Failure Analysis Case Histories: Processing Errors and Defects
2219 and Alclad 2219 High-Temperature Alloy
Properties and Selection of Aluminum Alloys