Abstract
Welded joints in any component or structure require a thorough inspection. The role of nondestructive evaluation (NDE) in the inspection of welds is very important, and the technology has become highly developed as a result. This article describes the applications, methods, evaluation procedures, performance, and limitations of NDE. It provides information on the training and certification of NDE operators, evaluation of test results, and guidance to method selection. Typical examples of various NDE methods for welds are also described.
You do not currently have access to this chapter.
Citation
Inspection and Evaluation of Weldments, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 85–109, https://doi.org/10.31399/asm.tb.wip.t65930085
Download citation file:
Related Book Content
Failure of a Cast Steel Crane Bolster
Handbook of Case Histories in Failure Analysis
Intergranular Cracking and Failure of Stainless Steel Vanes from a Closed, Riveted Impeller
Handbook of Case Histories in Failure Analysis
Failure Analysis Methodology
Failure Analysis of Engineering Structures Methodology and Case Histories
Electromagnetic Acoustic Transducers for Nondestructive Evaluation
Nondestructive Evaluation of Materials
Metallography and Microstructures of Weldments
Metallography and Microstructures
Guide to Nondestructive Evaluation Techniques
Nondestructive Evaluation of Materials
Nondestructive Evaluation of Solid-State Welds
Nondestructive Evaluation of Materials
Inspection of Powder Metallurgy Parts
Inspection of Metals Understanding the Basics
Phased Array Ultrasound
Nondestructive Evaluation of Materials