Book Chapter
Chapter 5: Cracking Phenomena Associated with Welding[1] Available to Purchase
By
Michael J. Cieslak
Michael J. Cieslak
Physical and Joining Metallurgy Department, Sandia National Laboratories
Search for other works by this author on:
-
Published:1997
Page range:
71 - 83
Abstract
The formation of defects in materials that have been fusion welded is a major concern in the design of welded assemblies. This article describes four types of defects that, in particular, have been the focus of much attention because of the magnitude of their impact on product quality. Colloquially, these four defect types are known as hot cracks, heat-affected zone microfissures, cold cracks, and lamellar tearing.
You do not currently have access to this chapter.
Citation
Michael J. Cieslak, Cracking Phenomena Associated with Welding, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 71–83, https://doi.org/10.31399/asm.tb.wip.t65930071
Download citation file:
Related Book Content
Influence of Welding on Steel Weldment Soundness
Welding, Brazing, and Soldering
Energy Sources Used for Fusion Welding
Welding, Brazing, and Soldering
Low-Carbon Structural Steels
Light Microscopy of Carbon Steels
Arc Welding of Carbon Steels
Welding, Brazing, and Soldering
Cracking Phenomena Associated With Welding
Welding, Brazing, and Soldering
Failure of a Truck Mounted Hydraulic Crane
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Failure of Ship Hull Plate Attributed to Lamellar Tearing
ASM Failure Analysis Case Histories: Offshore, Shipbuilding, and Marine Equipment
Brittle Failure of a Pressure Vessel After Welded Modifications Without Stress-Relief Heat Treatment
ASM Failure Analysis Case Histories: Chemical Processing Equipment
Welding
Light Microscopy of Carbon Steels
Welding Process Fundamentals
Welding Fundamentals and Processes