Discontinuities are interruptions in the desirable physical structure of a weld. This article describes the types of weld discontinuities that are characteristic of the principal welding processes. Discontinuities covered are metallurgical discontinuities, discontinuities associated with specialized welding processes, and base metal discontinuities. In addition, information on the common inspection methods used to detect these discontinuities is provided.