Weld Integrity and PerformanceAvailable to Purchase
Weld Integrity and Performance is a convenient reference and sourcebook for anyone involved in the application, fabrication, or assessment of welded structures. It provides detailed information on relevant topics including weld solidification, weldability testing, weld characterization, discontinuities and imperfections, cracking phenomena, inspection and evaluation techniques, fatigue and fracture control, fracture mechanics, fitness-for-service testing, repair welding, and weld corrosion. An entire section, the largest by far in the book, covers the basic metallurgy and engineering properties of weldments made from carbon and low-alloy steels, stainless steels, aluminum alloys, titanium alloys, nickel-base alloys, and refractory metals, including tantalum, niobium, molybdenum, and tungsten alloys. The book also provides insights into the origins of failure associated with different welding processes and includes an appendix with information on the weldability of common alloys (including cast irons) as well as process selection guidelines, recommended preheat and interpass temperatures and postweld heat treatments for pipe welds and pressure vessels, and qualification codes and standards. For information on the print version, ISBN 978-0-87170-600-8, follow this link.
Download citation file:
Table of Contents
-
Introduction
-
Weld Imperfections and Cracking
-
Chapter 3: Characterization of Welds[1]ByCraig B. Dallam;Craig B. DallamThe Lincoln Electric CompanySearch for other works by this author on:Brian K. DamkrogerBrian K. DamkrogerSandia National LaboratoriesSearch for other works by this author on:Published:01 July 1997
-
Chapter 5: Cracking Phenomena Associated with Welding[1]ByMichael J. CieslakMichael J. CieslakPhysical and Joining Metallurgy Department, Sandia National LaboratoriesSearch for other works by this author on:Published:01 July 1997
-
-
Weld Failure Analysis and Prevention
-
Chapter 7: Fatigue and Fracture Control of Welds[1]ByPublished:01 July 1997
-
Chapter 8: Factors Influencing Weldment Fatigue[1]ByW.H. MunseW.H. MunseUniversity of Illinois at Urbana-ChampaignSearch for other works by this author on:Published:01 July 1997
-
Chapter 10: Repair Welding[1]ByRobert J. DybasRobert J. DybasGeneral Electric CompanySearch for other works by this author on:Published:01 July 1997
-
Chapter 11: Corrosion of Weldments[1]ByC.E. CrossC.E. CrossMartin Marietta Astronautics GroupSearch for other works by this author on:Published:01 July 1997
-
-
Engineering Properties of Welds
-
Reference Information