Abstract
Hardenability refers to the ability of steel to obtain satisfactory hardening to some desired depth when cooled under prescribed conditions. It is governed almost entirely by the chemical composition (carbon and alloy content) at the austenitizing temperature and the austenite grain size at the moment of quenching. This article describes the Jominy end-quench test, the Grossman method, and the air hardenability test to evaluate hardenability. It also reviews the factors that influence steel hardenability and selection.
Sign in
ASM members
Member Sign InHardness and Hardenability of Steels, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 26–59, https://doi.org/10.31399/asm.hb.v04a.a0005823
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.