Steel Heat Treating Fundamentals and Processes
Introduction to Steel Heat Treatment[1]
-
Published:2013
Abstract
The heat treatment of steel is based on the physical metallurgical principles that relate to its processing, properties, and structure. The microstructures that result from the heat treatment of steel are composed of one or more phases in which the atoms of iron, carbon, and other elements in steel are associated. This article describes the phases of heat treated steel, and provides information on effect of temperature change and the size of carbon atoms relative to that of iron atoms during the heat treatment.
Sign in
ASM members
Member Sign InIntroduction to Steel Heat Treatment, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 3–25, https://doi.org/10.31399/asm.hb.v04a.a0005819
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.