Electrical Testing and Characterization of Plastics
-
Published:2022
Abstract
This article addresses electrical testing and characterization of plastics and presents a number of techniques for evaluating the electrical properties of insulating materials, with a special focus on plastics, accompanied by a list of the electrical properties of different types of plastics. It provides the reader with sufficient information to select the appropriate electrical test(s) for a specific application. The tests covered in this article are widely used in industry to determine the electrical properties of insulating materials, particularly plastics. The article lists and defines terms used in connection with testing and specification of plastics for electrical applications.
Abdullahi Abubakar Mas’ud, Electrical Testing and Characterization of Plastics, Characterization and Failure Analysis of Plastics, Vol 11B, ASM Handbook, Edited By Todd J. Menna, ASM International, 2022, p 219–230, https://doi.org/10.31399/asm.hb.v11B.a0006913
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!