Rheological Testing of Polymers
By
Gregory W. Kamykowski
Gregory W. Kamykowski
TA Instruments – Waters LLC
Search for other works by this author on:
-
Published:2022
Abstract
Rheology is defined as the study of the flow and deformation of matter. This article begins with an examination of flow behavior. It describes the geometries and methods employed for rheological testing of polymers in their molten state. It also discusses materials that are predominantly in the solid state and the methods employed for solids testing. Examples of unidirectional and dynamic oscillatory testing are provided for different mechanical behaviors.
Topics
Chemical analysis,
Polymer degradation,
Polymers,
Polymer processing,
Chemical composition,
Engineering design,
Materials selection,
Root cause analysis,
Thermal analysis,
Rheological testing,
Polymers,
Flow,
Chemical analysis,
Polymer degradation,
Polymers,
Polymer processing,
Chemical composition,
Engineering design,
Materials selection,
Root cause analysis,
Thermal analysis
You do not currently have access to this chapter.
Citation
Gregory W. Kamykowski, Rheological Testing of Polymers, Characterization and Failure Analysis of Plastics, Vol 11B, ASM Handbook, Edited By Todd J. Menna, ASM International, 2022, p 157–172, https://doi.org/10.31399/asm.hb.v11B.a0006930
Download citation file:
Related Book Content
Fracture of Plastics
Characterization and Failure Analysis of Plastics
Material Jetting of Polymers
Additive Manufacturing Processes
Powder Bed Fusion of Polymers
Additive Manufacturing Processes
Differential Scanning Calorimetry
Materials Characterization (2019 Edition)
Flammability Testing
Characterization and Failure Analysis of Plastics
Design for Deformation Processing
Metalworking: Bulk Forming
Analysis of Distortion and Deformation
Failure Analysis and Prevention (2021 Edition)
Introduction to the Mechanical Behavior of Nonmetallic Materials
Mechanical Testing and Evaluation
Introduction
Binder and Polymer Assisted Powder Processing
Glossary
Binder and Polymer Assisted Powder Processing