Characterization and Failure Analysis of Plastics
Environmental Stress Cracking
-
Published:2022
Abstract
While there are many fracture mechanisms that can lead to the failure of a plastic component, environmental stress cracking (ESC) is recognized as one of the leading causes of plastic failure. This article focuses on unpacking the basic concepts of ESC to provide the engineer with a better understanding of how to evaluate and prevent it. It then presents factors that affect and contribute to the susceptibility of plastic to ESC: material factors, chemical factors, stress, and environmental factors. The article includes the collection of background information to understand the circumstances surrounding the failure, a fractographic evaluation to assess the cracking, and analytical testing to evaluate the material, design, manufacturing, and environmental factors.
Javier C. Cruz, Jeffrey A. Jansen, Environmental Stress Cracking, Characterization and Failure Analysis of Plastics, Vol 11B, ASM Handbook, Edited By Todd J. Menna, ASM International, 2022, p 1–15, https://doi.org/10.31399/asm.hb.v11B.a0006917
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.