Hardness Testing: Principles and Applications
Edited by
ASM International
ISBN electronic:
978-1-62708-346-1
Publication date:
2011
Abstract
This chapter reviews the general principles involved in codifying standards and describes the historical development of materials testing standards. It provides information on the standards related to the Brinell, Vickers, Rockwell, and Knoop methods as well as those for the instrumented indentation test and hardness conversions.
You do not currently have access to this chapter.
Citation
A. Wehrstedt, Standardization, Hardness Testing: Principles and Applications, Edited By Konrad Herrmann, ASM International, 2011, p 235–246, https://doi.org/10.31399/asm.tb.htpa.t53310235
Download citation file:
Related Book Content
Hardness Measurement of Metals—Static Methods
Hardness Testing Principles and Applications
Hardness Testing
Inspection of Metals Understanding the Basics
Macroindentation Hardness Testing
Mechanical Testing and Evaluation
Instrumented Indentation Test
Hardness Testing Principles and Applications
Introduction to Hardness Testing
Mechanical Testing and Evaluation