Abstract
Instrumented indentation hardness testing significantly expands on the capabilities of traditional hardness testing. It employs high-resolution instrumentation to continuously control and monitor the loads and displacements of an indenter as it is driven into and withdrawn from a material. The scope of application comprises displacements even smaller than 200 nm (nano range) and forces even up to 30 kN . Mechanical properties are derived from the indentation load-displacement data obtained in simple tests. The chapter presents the elements of contact mechanics that are important for the application of the instrumented indentation test. The test method according to the international...
Sign in
ASM members
Member Sign InC. Ullner, Instrumented Indentation Test, Hardness Testing: Principles and Applications, Edited By Konrad Herrmann, ASM International, 2011, p 167–233, https://doi.org/10.31399/asm.tb.htpa.t53310167
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.