This chapter describes the procedures, characteristics, and applications for static hardness test methods. It addresses test methods that are state of the art, commonly used, or that may find increased use due to certain advantages. The methods addressed are Rockwell hardness testing (ISO 6508 and ASTM E 18), Vickers hardness testing (ISO 6507, ASTM E92, and ASTM E384), Brinell hardness testing (ISO 6506 and ASTM E10), and Knoop hardness testing (ISO 4545 and ASTM E284). The chapter also discusses the advantages and disadvantages of these test methods.