Pipeline Failure Results from Lightning Strike: Act of Mother Nature?
-
Published:2019
Abstract
A section of pipe in a hydrocarbon pipeline was found to be leaking. The pipeline was installed several decades earlier and was protected by an external coating of extruded polyethylene and a cathodic protection system. The failed pipe section was made from API 5L X46 line pipe steel, approximately 22 cm (8.7 in.) OD x 0.5 cm (0.2 in.) wall thickness, which was electric resistance welded along the longitudinal seam. The pressure at the time and location of the failure was 2760 kPa, which corresponds to 20% of the specified minimum yield strength. The cause of failure (based on visual inspection, magnetic particle inspection, stereoscopic analysis, scanning electron microscopy, tensile and hardness testing, and chemical analysis) was attributed to damage resulting from a lightning strike.
G.T. Quickel, J.A. Beavers, Pipeline Failure Results from Lightning Strike: Act of Mother Nature?, Handbook of Case Histories in Failure Analysis, Vol 3, Edited By Larry Berardinis, ASM International, 2019, p 496–500, https://doi.org/10.31399/asm.fach.v03.c9001823
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.