Handbook of Case Histories in Failure Analysis
Abstract
An ASTM A391 steel chain link of an over head hoist failed catastrophically, causing damage to both property and personnel. Macrofractography identified the sequence of fractures within the chain link. The first fracture occurred at the welded joint, a second occurred opposite the weld. SEM fractography and metallography indicated that the link failed in a ductile manner because of tensile overload, which occurred when the hoist hook contacted the hoist's housing and prevented uptake of the chain. It was recommended that a load-sensing device be installed to prevent future occurrences and that a dye penetrant inspection be performed on...
Sign in
ASM members
Member Sign InArvid A. Casler, Tensile Failure of a Hoist Chain Link, Handbook of Case Histories in Failure Analysis, Vol 1, Edited By Khlefa A. Esaklul, ASM International, 1992, p 452–455, https://doi.org/10.31399/asm.fach.v01.c9001134
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!