Failure of a Type 317L Stainless Steel Clad Bottom Cone of an Acid Sulfite Pulping Batch Digester
By
Durgam G. Chakrapani
Durgam G. Chakrapani
MEI-Charlton, Inc.
Search for other works by this author on:
-
Published:1992
Abstract
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Durgam G. Chakrapani, Failure of a Type 317L Stainless Steel Clad Bottom Cone of an Acid Sulfite Pulping Batch Digester, Handbook of Case Histories in Failure Analysis, Vol 1, Edited By Khlefa A. Esaklul, ASM International, 1992, p 198–200, https://doi.org/10.31399/asm.fach.v01.c9001069
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Stress Corrosion Cracking Failures in Components Made of Austenitic Chromium Nickel Steels
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Transgranular Stress-Corrosion Cracking Failures in AISI 304L Stainless Steel Dished Ends During Storage
Handbook of Case Histories in Failure Analysis
Intergranular Stress-Corrosion Cracking of Carbon Steel Pipe Welds in a Kamyr Continuous Digester Equalizer Line
Handbook of Case Histories in Failure Analysis
Corrosion and Cracking of the Internal Surfaces of a Black Liquor Digester
Handbook of Case Histories in Failure Analysis
Thermal Spray Applications in the Paper Production Industry
Thermal Spray Technology
Guidelines for Maintenance Coating of Steel Structures in Pulp and Paper Mills
Protective Organic Coatings
Intergranular Corrosion/Cracking of a Stainless Steel Pipe Reducer Section in Bleached Pulp Stock Service
Handbook of Case Histories in Failure Analysis
Stress-Corrosion Cracking of Nickel-Base Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking of Titanium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Mechanisms of Stress-Corrosion Cracking
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)