Alloy Cast Irons
Revising author
Revising author
-
Published:1990
Abstract
Alloy cast irons are considered to be those casting alloys based on the iron-carbon-silicon system that contain one or more alloying elements intentionally added to enhance one or more useful properties. Alloy cast irons can be classified as white cast irons, corrosion-resistant cast irons, and heat-resistant cast irons. This article discusses abrasion-resistant chilled and white irons, high-alloy corrosion-resistant irons, and medium-alloy and high-alloy heat-resistant gray and ductile irons. The article outlines in a list the approximate ranges of alloy content for various types of alloy cast irons. The article explains the effects of alloying elements and the effects of inoculants. In most cast irons, it is the interaction among alloying elements that has the greatest effect on properties. Inoculants other than appropriate graphitizing or nodularizing agents are used rarely, if ever, in high-alloy corrosion-resistant or heat-resistant irons.
Richard B. Gundlach, Douglas V. Doane, Alloy Cast Irons, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 85–104, https://doi.org/10.31399/asm.hb.v01.a0001006
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.