Malleable iron possesses considerable ductility and toughness because of its combination of nodular graphite and a low-carbon metallic matrix. The desired formation of temper carbon in malleable irons has two basic requirements. First, graphite should not form during the solidification of the white cast iron, and second, graphite must also be readily formed during the annealing heat treatment. These two metallurgical requirements influence the useful compositions of malleable irons and the melting, solidification, and annealing procedures. There are two basic types of malleable iron: blackheart and whiteheart. This article considers only the blackheart type and describes the metallurgical factors of malleable iron. It discusses the mechanical properties of pearlitic and martensitic malleable irons. The article provides additional information on the properties and heat treatment of ferritic, pearlitic, and martensitic malleable irons. The article lists some of the typical applications of malleable iron castings.
Malleable Iron, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 71–84, https://doi.org/10.31399/asm.hb.v01.a0001005
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.