Properties and Selection: Irons, Steels, and High-Performance Alloys
Steel Processing Technology
-
Published:1990
Abstract
This article describes ironmaking and steelmaking practices (melt or liquid processing, including hot metal desulfurization) and discusses the evolution of these processes and their effects on steel properties. The physical chemistry of steelmaking may appear deceptively simple for integrated steel mill operations where ore from the ground is converted into steel. The various refining steps that occur in steelmaking are reviewed. The article also describes solid processing of steel, with emphasis on hot and cold rolling, thermomechanical processing, and annealing of flat steel products.
R.I.L. Guthrie, J.J. Jonas, Steel Processing Technology, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 107–125, https://doi.org/10.31399/asm.hb.v01.a0001007
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.