Properties and Selection: Irons, Steels, and High-Performance Alloys
High-Strength Structural and High-Strength Low-Alloy Steels
-
Published:1990
Abstract
This article considers four types of high-strength structural steels: heat-treated low-alloy steels, as-rolled carbon-manganese steels, heat-treated (normalized or quenched and tempered) carbon steels, and as-rolled high-strength low-alloy (HSLA) steels (which are also known as microalloyed steels). The article places emphasis on HSLA steels, which are an attractive alternative in structural applications because of their competitive price per-yield strength ratios. HSLA steels are primarily hot-rolled into the usual wrought product forms and are furnished in the as-hot-rolled condition. In addition to hot-rolled products, HSLA steels are also furnished as cold-rolled sheet and forgings. This article describes the different categories of HSLA steels and provides a summary of characteristics and intended uses of HSLA steels described in the American Society for Testing and Materials (ASTM) specifications. The article also presents some applications of HSLA steels.
High-Strength Structural and High-Strength Low-Alloy Steels, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 389–423, https://doi.org/10.31399/asm.hb.v01.a0001025
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.