Abstract
Stainless steels are widely used at elevated temperatures when carbon and low-alloy steels do not provide adequate corrosion resistance and/or sufficient strength at these temperatures. This article deals with the wrought stainless steels used for high temperature applications. It gives some typical compositions of wrought heat-resistant stainless steels, which are grouped into ferritic, martensitic, austenitic, and precipitation-hardening (PH) grades. Quenched and tempered martensitic stainless steels are essentially martensitic and harden when air cooled from the austenitizing temperature. These alloys offer good combinations of mechanical properties. The article focuses on mechanical property considerations and corrosion resistance considerations of stainless steels. The corrosion and oxidation resistance of wrought stainless steels is similar to that of cast stainless steels with comparable compositions.
Elevated-Temperature Properties of Stainless Steels, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 930–949, https://doi.org/10.31399/asm.hb.v01.a0001048
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.