Properties and Selection: Irons, Steels, and High-Performance Alloys
Threaded Steel Fasteners
-
Published:1990
Abstract
This article discusses the properties of threaded fasteners made from carbon and low-alloy steels containing a maximum of 0.55% carbon. It provides guidelines for the selection of steels for bolts, studs, and nuts intended for use at temperatures between -50 and 370 deg C. The article also discusses steels rated for service above 370 deg C and describes internationally recognized grade designations. The specifications provided can be used to outline fastener requirements, control manufacturing processes, and establish functional or performance standards. The most commonly used protective metal coatings for ferrous metal fasteners; zinc, cadmium, and aluminum; are described as well.
ASM Committee on Threaded Steel Fasteners , Frank W. Akstens, James Gialamas, Edward J. Bueche, T.P. Madvad, Brian Murkey, Joseph McAuliffe, Gregory D. Sander, Edwin F. Frederick, Hal L. Miller, P.C. Hagopian, James Fox, Threaded Steel Fasteners, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 289–301, https://doi.org/10.31399/asm.hb.v01.a0001018
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.