Handbook of Case Histories in Failure Analysis
Leaks in Copper Tubing From Cooling Coils of a Large Air-Conditioning Unit
-
Published:1993
Abstract
Copper tubes from the cooler assemblies of a large air-conditioning unit exhibited leakage upon installation of the unit. Sections from two leaking tubes and one nonleaking tube were subjected to pressure testing and microscopic examination. The cause of leaking was determined to be pitting corrosion. Extensive pitting was found on the insides of all sections examined, with deep and numerous pits in leaking areas. Circumstantial evidence indicated that antifreeze solution left in the tubes from the manufacturing operation was the most likely cause of the pitting.
Sign in
ASM members
Member Sign InJ.O. Edwards, R.I. Hamilton, Leaks in Copper Tubing From Cooling Coils of a Large Air-Conditioning Unit, Handbook of Case Histories in Failure Analysis, Vol 2, Edited By Khlefa A. Esaklul, ASM International, 1993, p 204–206, https://doi.org/10.31399/asm.fach.v02.c9001338
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.