Abstract
This appendix contains tables listing the approximate composition of materials for the extrusion process. The materials covered are aluminum alloys, magnesium and magnesium alloys, copper and copper alloys, cobalt alloys, nickel and nickel alloys, iron alloys, steels, lead, tin, zinc alloys, molybdenum, niobium, tantalum, zirconium alloys, titanium, and titanium alloys.
Topics
Extrusion dies,
Extruders,
Hot billet handling systems,
Billets,
Extrusions,
Seamless metal tubes,
Hot melt extrusion,
Thermomechanical analysis,
Extrusion welding,
Extrusion,
Powder extrusion,
Bulk formability,
Deformation modeling,
Compressive properties,
Friction and wear properties,
Ductility,
Flow stress,
Plastic strain,
Strain rate,
Plastic flow,
Temperature,
Work and tool-holding devices,
Quality planning tools,
Ferrous metals and alloys,
Nonferrous metals and alloys,
Chemical composition
You do not currently have access to this chapter.
Citation
Approximate Composition of Materials, Extrusion, 2nd ed., By A.F. Castle;Edited By M. Bauser, G. Sauer, K. Siegert, ASM International, 2006, p 567–577, https://doi.org/10.31399/asm.tb.ex2.t69980567
Download citation file:
Related Book Content
General Introduction to Casting
Metals Handbook Desk Edition (2nd Edition)
The Production of Extruded Semifinished Products from Metallic Materials
Extrusion (Second Edition)
Vapor Phase Corrosion Inhibitors
Corrosion: Fundamentals, Testing, and Protection
Inclusion-Forming Reactions
Casting
Guide to Materials Selection
Engineered Materials Handbook Desk Edition
Corrosion in Petroleum Refining and Petrochemical Operations
Corrosion: Environments and Industries
Research and Development
Aluminum Extrusion Technology
Hydrogen Damage
Corrosion: Fundamentals, Testing, and Protection
Thermodynamics in Extrusion
Aluminum Extrusion Technology
Extrusion Press and Auxiliary Equipment
Aluminum Extrusion Technology