Abstract
This chapter provides an overview of the basic principles and historic development of metal extrusion processes. It starts by illustrating the two major process categories: direct extrusion and indirect extrusion. It then briefly defines hydrostatic extrusion and the conform process. The history coverage addresses early patents for extrusion of lead at the turn of the 17th century up through the major process innovations in the 20th century.
You do not currently have access to this chapter.
Citation
Introduction, Extrusion, 2nd ed., By A.F. Castle;Edited By M. Bauser, G. Sauer, K. Siegert, ASM International, 2006, p 1–7, https://doi.org/10.31399/asm.tb.ex2.t69980001
Download citation file:
Related Book Content
Extrusion
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Conventional Hot Extrusion
Metalworking: Bulk Forming
Tribology of Extrusion
Friction, Lubrication, and Wear Technology
Hydrostatic Extrusion of Metals and Alloys
Metalworking: Bulk Forming