This appendix provides readers with worked solutions to 25 problems involving calculations associated with tensile testing and the determination of mechanical properties and variables. The problems deal with engineering factors and considerations such as stress and strain, loading force, sample lengthening, and machine stiffness, and with mechanical properties and parameters such as elastic modulus, Young’s modulus, strength coefficient, strain-hardening exponent, and modulus of resilience. They also cover a wide range of materials including various grades of aluminum and steel as well as iron, titanium, brass, and copper alloys.