This chapter reviews the development of filament winding systems and the automated processes used in state-of-the-art filament winding facilities. It first provides a description on the early stages of modern filament winding, followed by brief information on the advances of filament winding in the computer age. Then, the chapter discusses the requirements for filament winding in manufacturing oil and gas industry components and in high-volume production of sporting goods, propane tanks, and curing ovens. The chapter concludes with examples of the versatility of filament winding in producing complex parts.
Sign in
ASM members
Member Sign InJohn E. Green, Automated Filament Winding Systems, Composite Filament Winding, Edited By S.T. Peters, ASM International, 2011, p 7–18, https://doi.org/10.31399/asm.tb.cfw.t52860007
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!