Chapter 14: Mechanical Joining by Forming
By
Deepak Rammohan
;
Deepak Rammohan
The Ohio State University
Search for other works by this author on:
Jose L. Gonzalez-Mendez
Jose L. Gonzalez-Mendez
The Ohio State University
Search for other works by this author on:
-
Published:2012
Abstract
This chapter describes joining by forming processes including riveting, clinching, crimping, and dieless joining techniques. It also discusses the fatigue behavior of clinched joints and the results of fatigue tests that compare clinched and spot welded joints.
Topics
Strain gauges,
Piezoelectric transducers,
Progressive dies,
Diffusion coating,
Plating,
Nitriding,
Clinching,
Crimping,
Riveting,
Blanking,
Bending,
Flow forming,
High-energy-rate forming,
Sheet forming,
Process modeling and simulation,
Eddy current inspection,
Forming equipment,
Wear testing,
Acoustic emission sensors,
Self-pierce riveting
You do not currently have access to this chapter.
Citation
Deepak Rammohan, Jose L. Gonzalez-Mendez, Mechanical Joining by Forming, Sheet Metal Forming: Processes and Applications, Edited By Taylan Altan, A. Erman Tekkaya, ASM International, 2012, p 289–300, https://doi.org/10.31399/asm.tb.smfpa.t53500289