Chapter 13: Incremental Sheet Forming
-
Published:2012
Abstract
This chapter describes incremental sheet forming processes, including single-point, two-point, and kinematic (two tool) techniques. It provides information on the tooling and equipment used, work flow and forming parameters, process mechanics and forming limits. It also discusses multistage forming strategies, process modeling and simulation, and advanced hybrid forming processes.
G. Hirt, M. Bambach, Incremental Sheet Forming, Sheet Metal Forming: Processes and Applications, Edited By Taylan Altan, A. Erman Tekkaya, ASM International, 2012, p 273–287, https://doi.org/10.31399/asm.tb.smfpa.t53500273