Indium and Bismuth
By
Laurence G. Stevens
;
Laurence G. Stevens
Indium Corporation of America
Search for other works by this author on:
C.E.T. White
C.E.T. White
Indium Corporation of America
Search for other works by this author on:
-
Published:1990
Abstract
This article focuses on the use of indium and bismuth in low-melting-temperature solders and fusible alloys. It describes how the two elements typically occur in nature and how they are recovered and processed for commercial use. It also provides information on designations, classification, composition, properties (including temperatures ranges), and some of the other ways in which indium and bismuth alloys are used.
You do not currently have access to this chapter.
Citation
Laurence G. Stevens, C.E.T. White, Indium and Bismuth, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 750–757, https://doi.org/10.31399/asm.hb.v02.a0001092
Download citation file:
Related Book Content
Failures in Soldering
Analysis and Prevention of Component and Equipment Failures
Soldering
Metals Handbook Desk Edition (2nd Edition)
Indium Plating
Surface Engineering
General Soldering
Welding, Brazing, and Soldering
Miscellaneous Nonferrous Metals
Elements of Metallurgy and Engineering Alloys
Machining of Stainless Steels
Machining
Copper and Copper Alloy Castings
Casting