Introduction
By
Małgorzata Warmuzek
Małgorzata Warmuzek
Foundry Research Institute
Search for other works by this author on:
-
Published:2016
Page range:
vii - xi
Abstract
This chapter provides an overview of the microstructure-property relationships associated with aluminum-silicon alloys. It includes information on commercial designations and grades, phase compositions, solidification paths, alloying elements, and intermetallic phases. It also provides solubility data and maps out the topics covered in subsequent chapters in the book.
You do not currently have access to this chapter.
Citation
Małgorzata Warmuzek, Introduction, Aluminum-Silicon Casting Alloys: Atlas of Microstructures, Edited By Malgorzata Warmuzek, ASM International, 2016, p vii–xi, https://doi.org/10.31399/asm.tb.ascaam.t59190vii
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Symbols, Abbreviations, and Intermetallic Phase Designations
Aluminum-Silicon Casting Alloys Atlas of Microstructures
Eutectic Alloy Systems
Phase Diagrams Understanding the Basics
Intermetallic Phases in Aluminum-Silicon Technical Cast Alloys
Aluminum-Silicon Casting Alloys Atlas of Microstructures
The Effects of Microstructure on Properties
Aluminum Alloy Castings Properties, Processes, and Applications
Resistance Brazing
Welding, Brazing, and Soldering
Failure of a Muffle for a Brazing Furnace
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Friction and Wear of Aluminum Alloys and Composites
Properties and Selection of Aluminum Alloys
Nickel and Nickel Alloys
Alloying Understanding the Basics
Selective Corrosion Attack at Brazed Joints
ASM Failure Analysis Case Histories: Processing Errors and Defects