Protective Organic Coatings
Abstract
The use of zinc in corrosion-protective coatings is due to its higher galvanic activity relative to that of steel. Pure zinc dust provides the best sacrificial protection to steel in a galvanic couple. Zinc-rich coatings can be subcategorized according to the type of binder material used, namely, inorganic and organic zinc-rich coatings. Common inorganic binders such as post-cured water-based alkali metal silicates, self-cured water-based alkali metal silicates, and self-cured solvent-based alkyl silicates, are reviewed. The article also compares inorganic and organic zinc-rich coatings, and discusses the concerns regarding zinc-rich coatings.
Kenneth B. Tator, Zinc-Rich Coatings, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 213–220, https://doi.org/10.31399/asm.hb.v05b.a0006049
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.