Chapter 22: Die Failures in Cold and Hot Forging Available to Purchase
By
-
Published:2005
Page range:
295 - 317
Abstract
This chapter addresses the issue of die failures in hot and cold forging operations. It describes failure classifications, fatigue fracture and wear mechanisms, analytical wear models, and the various factors that limit die life. It also includes several case studies in which finite-element modeling is used to predict die failure and extend die life.
You do not currently have access to this chapter.
Citation
Mark Gariety, Die Failures in Cold and Hot Forging, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 295–317, https://doi.org/10.31399/asm.tb.chffa.t51040295
Download citation file:
Related Book Content
Lubrication and Wear in Forging
Friction, Lubrication, and Wear Technology
Friction and Lubrication
Cold and Hot Forging Fundamentals and Applications
Failure in Steel Forging
Failure Analysis of Heat Treated Steel Components
Forging
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Hot Upset Forging
Metalworking: Bulk Forming
Process Modeling in Cold Forging Using Finite-Element Analysis
Cold and Hot Forging Fundamentals and Applications
Finite Element Method Applications in Bulk Forming
Metalworking: Bulk Forming
Cold and Warm Forging
Cold and Hot Forging Fundamentals and Applications
Finite-Element Modeling in Failure Analysis
Failure Analysis and Prevention (2021 Edition)
Extrusion Die and Tooling
Aluminum Extrusion Technology, Second Edition