Chapter 18: Process Modeling in Cold Forging Using Finite-Element Analysis
-
Published:2005
Abstract
This chapter discusses the use of finite-element methods for modeling cold forging processes. The discussion covers process modeling inputs, such as geometric parameters, material properties, and interface conditions, and includes several application examples.
Topics
Fracture analysis,
Extrusion dies,
Forging dies,
Forging machines,
Metal forming lubricants,
Wrought superalloys,
Billets,
Forgings,
Shearing,
Backward extrusion,
Forward extrusion,
Cold forging,
Die forging,
Hot forging,
Hammer forging,
Press forging,
Radial forging,
Ring forging,
Roll forging,
Rotary forging,
Finite element analysis,
Microstructure modeling,
Forgeability,
Friction and wear properties,
Flow stress,
Plane stress,
Plastic strain,
Engineering strain,
Lubricant analysis,
Coefficient of friction
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Prashant Mangukia, Process Modeling in Cold Forging Using Finite-Element Analysis, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 237–246, https://doi.org/10.31399/asm.tb.chffa.t51040237
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Process Modeling in Impression-Die Forging Using Finite-Element Analysis
Cold and Hot Forging Fundamentals and Applications
Friction and Lubrication
Cold and Hot Forging Fundamentals and Applications
Cold and Warm Forging
Cold and Hot Forging Fundamentals and Applications
Failure in Steel Forging
Failure Analysis of Heat Treated Steel Components
Isothermal and Hot-Die Forging
Metalworking: Bulk Forming
Glossary of Terms: Modeling for Metals Processing
Fundamentals of Modeling for Metals Processing
Die Failures in Cold and Hot Forging
Cold and Hot Forging Fundamentals and Applications
Models for Fracture during Deformation Processing
Fundamentals of Modeling for Metals Processing
Modeling of Residual Stress and Machining Distortion in Aerospace Components
Metals Process Simulation
Process Modeling
Thermal Spray Technology