Chapter 16: Process Modeling in Impression-Die Forging Using Finite-Element Analysis
-
Published:2005
Abstract
This chapter discusses the use of finite-element modeling in forging design. It describes key modeling parameters and inputs, mesh generation and computation time, and process modeling outputs such as metal flow, strain rate, loading profiles, and microstructure. It also includes a variety of application examples.
Manas Shirgaokar, Gracious Ngaile, Gangshu Shen, Process Modeling in Impression-Die Forging Using Finite-Element Analysis, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 193–209, https://doi.org/10.31399/asm.tb.chffa.t51040193