Chapter 9: Methods of Analysis for Forging Operations
-
Published:2005
Abstract
There are numerous approximate methods, both analytical and numerical, for analyzing forging processes. None are perfect because of the assumptions made to simplify the mathematical approach, but all have merit. This chapter discusses the slab, upperbound, and finite element methods, covering basic principles, implementation, and advantages and disadvantages in various applications.
Topics
Fracture analysis,
Extrusion dies,
Forging dies,
Forging machines,
Metal forming lubricants,
Wrought superalloys,
Billets,
Forgings,
Shearing,
Backward extrusion,
Forward extrusion,
Cold forging,
Die forging,
Hot forging,
Hammer forging,
Press forging,
Radial forging,
Ring forging,
Roll forging,
Rotary forging,
Finite element analysis,
Microstructure modeling,
Forgeability,
Friction and wear properties,
Flow stress,
Plane stress,
Plastic strain,
Engineering strain,
Lubricant analysis,
Forging,
Plane strain
You do not currently have access to this chapter.
Citation
Manas Shirgaokar, Methods of Analysis for Forging Operations, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 91–105, https://doi.org/10.31399/asm.tb.chffa.t51040091
Download citation file:
Related Book Content
Deep Drawing of Round and Rectangular Cups
Sheet Metal Forming Fundamentals
Modeling of Deformation Processes—Slab and Upper Bound Methods
Fundamentals of Modeling for Metals Processing
Models for Fracture during Deformation Processing
Fundamentals of Modeling for Metals Processing
Principles of Forging Machines
Cold and Hot Forging Fundamentals and Applications
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Temperature and Heat Transfer
Cold and Hot Forging Fundamentals and Applications
Primary Working
Titanium Physical Metallurgy, Processing, and Applications
Forging and Forming
Superalloys: A Technical Guide (Second Edition)
Casting, Forming, and Forging
Gear Materials, Properties, and Manufacture
Forging Design Involving Draft
Metalworking: Bulk Forming