Cold and Hot Forging: Fundamentals and Applications
Edited by
ASM International
ISBN electronic:
978-1-62708-300-3
Publication date:
2005
Book Chapter
Chapter 6: Temperature and Heat Transfer
By
-
Published:2005
Page range:
59 - 66
Abstract
This chapter discusses the factors that influence temperature in forging operations and presents equations that can be used to predict and control it. The discussion covers heat generation and transfer, the effect of metal flow, temperature measurement, testing methods, and the influence of equipment-related parameters such as press speed, contact time, and tooling geometries.
You do not currently have access to this chapter.
Citation
Gangshu Shen, Temperature and Heat Transfer, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 59–66, https://doi.org/10.31399/asm.tb.chffa.t51040059
Download citation file:
Related Book Content
Principles of Forging Machines
Cold and Hot Forging Fundamentals and Applications
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Glossary: Bulk Forming
Metalworking: Bulk Forming
Forging Design Involving Draft
Metalworking: Bulk Forming
Forging Design Involving Flash and Trim
Metalworking: Bulk Forming
Forging and Forming
Superalloys: A Technical Guide (Second Edition)
Aluminum Forging
Aluminum: Technology, Industry, and Applications
Casting, Forming, and Forging
Gear Materials, Properties, and Manufacture
Primary Working
Titanium Physical Metallurgy, Processing, and Applications
Salt Solutions as Quenchants
Quenchants and Quenching Technology