Beryllium-related lung diseases were first reported in the 1930s, several years after the emergence of beryllium metals in manufactured products. Since then, there have been numerous studies around the world and continued refinement of recommendations and safety standards. This chapter provides a summary of the studies that have been conducted along with the findings. It discusses the effects of acute and chronic exposure, toxicity levels, potential sources and risks, treatment, and protective and preventive measures.