Chapter 16: Metallography of Beryllium and Beryllium Alloys
By
Edgar E. Vidal
Edgar E. Vidal
Brush Wellman, Inc.
Search for other works by this author on:
-
Published:2009
Page range:
199 - 208
Abstract
This chapter explains how to safely prepare beryllium alloy samples for metallographic analysis. It describes grinding, polishing, and etching procedures in detail. It also discusses the identification of major and minor constituents and the general appearance of beryllium microstructure.
You do not currently have access to this chapter.
Citation
David L. Olson, Edgar E. Vidal, Metallography of Beryllium and Beryllium Alloys, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 199–208, https://doi.org/10.31399/asm.tb.bcp.t52230199
Download citation file:
Related Book Content
Medical Aspects of the Toxicity of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
High-Temperature Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Metallography and Microstructures of Powder Metallurgy Alloys
Metallography and Microstructures
Welding and Joining of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Aqueous Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Beryllium Binary Phase Diagrams
Beryllium Chemistry and Processing
Machining of Beryllium
Machining
History of Beryllium
Beryllium Chemistry and Processing
Metallography and Microstructures of Beryllium, Copper-Beryllium, and Nickel-Beryllium Alloys
Metallography and Microstructures
Metallography
Inspection of Metals Understanding the Basics