Abstract
This chapter is a compilation of beryllium phase diagrams, representing more than 25 binary alloy systems from beryllium-aluminum to beryllium-zirconium. Each diagram is presented along with a summary and source reference.
You do not currently have access to this chapter.
Citation
Loren A. Jacobson, Beryllium Binary Phase Diagrams, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 179–197, https://doi.org/10.31399/asm.tb.bcp.t52230179
Download citation file:
Related Book Content
Introduction to Phase Diagrams
Phase Diagrams Understanding the Basics
High-Temperature Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Medical Aspects of the Toxicity of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Welding and Joining of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Metallography of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Aqueous Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Intermediate Phases
Alloy Phase Diagrams
Beryllium and Aluminum-Beryllium Alloys
Powder Metallurgy
Brazing of Refractory and Reactive Metals
Welding, Brazing, and Soldering