This chapter provides an overview of the physical metallurgy of beryllium, discussing phases and phase transformations, physical and mechanical properties, heat treatment, and alloying. It explains how the atomic structure of beryllium, particularly its sp hybrid state, contributes to the anisotropy of elastic constants and slip properties, resulting in a specific stiffness, or modulus-to-density ratio, six times higher than that of any other structural material.