Abstract
This chapter describes some of the chemical processes that have been developed to extract beryllium from different types of ore. It covers the Kjellgren-Sawyer sulfate method, the Degussa method, Copaux-Kawecki fluoride extraction, solvent extraction, and leaching and settling. It also provides information on electrolytic extraction and the use of electrorefining.
You do not currently have access to this chapter.
Citation
Kenneth A. Walsh, Edgar E. Vidal, Brajendra Mishra, Extractive Metallurgy, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 71–92, https://doi.org/10.31399/asm.tb.bcp.t52230071
Download citation file:
Related Book Content
History of Beryllium
Beryllium Chemistry and Processing
Introduction
Beryllium Chemistry and Processing
Amorphous Alloys That Contain Beryllium
Beryllium Chemistry and Processing
Hygienic Practices for Handling Beryllium and Its Components
Beryllium Chemistry and Processing
Chemistry of Beryllium
Beryllium Chemistry and Processing
Metal Removal
Beryllium Chemistry and Processing
Beryllium Waste Recycling
Beryllium Chemistry and Processing
Sources of Beryllium
Beryllium Chemistry and Processing
Powder Metallurgy
Beryllium Chemistry and Processing
High-Temperature Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing