Abstract
This chapter describes some of events and developments that helped drive the commercialization of beryllium and its acceptance as an engineering material. It traces the growth of the domestic beryllium industry from its origins in the 1920s to the present time, and provides a status update on the primary beryllium producers throughout the world.
Kenneth A. Walsh, Donald J. Kaczynski, Loren A. Jacobson, David L. Olson, History of Beryllium, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 7–18, https://doi.org/10.31399/asm.tb.bcp.t52230007
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.